Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of FLEX NORYL™ Resin WCD915 - Asia - (PPE+TPE) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for FLEX NORYL™ Resin WCD915 - Asia:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Flex Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
FLEX NORYL™ WCD915 resin is a flexible, UV stabilized, non-reinforced extrudable blend of Polyphenylene Ether (PPE) + Thermoplastic Elastomer (TPE). This material contains non-halogenated flame retardant and performance capable of meeting UL 1581 VW-1 requirement and 90C or 105C end use temperature rating as defined by UL 62 TPE category. FLEX NORYL WCD915 resin is intended for evaluation in wire and cable applications such as cable insulation materials. It has a Shore A Hardness reading of 91 and exhibits superior thermal stability, very low water absorption, good electric properties, and low specific gravity. Processing is typically conducted on standard extrusion equipment, and UL 1581 testing is conducted on 2.0mm wire with 0.12mm X 20 stranded copper conductor.
Processing/Physical Characteristics単位テスト基準
ASTM数据
メルトフローレイト, MFI 9 g/10min ASTM D 1238
温度 250 °C -
荷重 10 kg -
機械的特性単位テスト基準
ISO データ
破壊応力 14 MPa ISO 527
破壊ひずみ 50 % ISO 527
ASTM数据
破壊応力 15 MPa ASTM D 638
破断伸び 170 % ASTM D 638
ショア硬さA 91 - ASTM D 2240
熱的特性単位テスト基準
ISO データ
グローワイヤ燃焼性指数 (GWFI) 960 °C IEC 60695-2-12
GWFI - 試験片の厚さ 3 mm -
グローワイヤ着火温度 (GWIT) 825 °C IEC 60695-2-13
GWIT - 試験片の厚さ 3 mm -
電気的特性.単位テスト基準
ISO データ
耐トラッキング性 600 - IEC 60112
ASTM数据
誘電正接, 1 MHz 0.033 - ASTM D 150
比誘電率, 1 MHz 2.6 - ASTM D 150
体積抵抗率 >1E15 Ohm*cm ASTM D 257
その他の特性.単位テスト基準
密度 1030 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Screw speed 15 - 85 rpm -
特殊な特性
添加剤.
難燃剤.
特殊な特性.
難燃.
領域別の利用可能性
アジア/太平洋地域.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.